The knowledge on the surface deviations and wear of recently introduced additively or subtractively manufactured materials indicated for definitive prosthesis is limited. The aim of this present study was to evaluate the external surface and mesiodistal width deviation and the occlusal surface wear of one additively manufactured composite resin (MS) and three subtractively manufactured resins (nanographene-reinforced polymethylmethacrylate (GR), conventional polymethylmethacrylate (PMMA), and reinforced composite resin (BC)) after thermomechanical aging. Molar-shaped crowns were fabricated in the tested materials and digitized with an intraoral scanner (CEREC Primescan; Dentsply Sirona, Bensheim, Germany). Each crown was subjected to thermomechanical aging and rescanned with the same scanner. A three-dimensional analysis software (Geomagic Control X v.2022.1; 3D Systems, Rock Hill, SC, USA) was used to calculate the deviations on the external surface, mesiodistal width, and wear on the occlusal surfaces of the tested crowns. Data were analyzed using one-way ANOVA and Tukey's tests (alpha = 0.05). MS had higher external surface deviations than PMMA and GR (p <= 0.038) and higher mesiodistal width deviations than PMMA and BC (p = 0.004). BC and GR had higher volume loss than PMMA (p <= 0.002). The additively manufactured composite resin was more prone to deviations, while reinforced composite resin had lower wear resistance than most of the tested materials.

Açıklama

Anahtar Kelimeler

Additive Manufacturing, External Deviation, Mesiodistal Width, Occlusal Wear, Thermomechanical Aging

Kaynak

Applied Sciences-Basel

WoS Q Değeri

N/A

Scopus Q Değeri

Cilt

13

Sayı

21

Künye