Load-to-failure resistance and optical characteristics of nano-lithium disilicate ceramic after different aging processes

dc.authoridMustafa Borga Dönmez / 0000-0002-3094-7487en_US
dc.authorscopusidMustafa Borga Dönmez / 57202022054
dc.authorwosidMustafa Borga Dönmez / AGY-6155-2022en_US
dc.contributor.authorDönmez, Mustafa Borga
dc.contributor.authorOlcay, Emin Orkun
dc.contributor.authorDemirel, Münir
dc.date.accessioned2022-06-28T07:06:24Z
dc.date.available2022-06-28T07:06:24Z
dc.date.issued2022en_US
dc.departmentİstinye Üniversitesi, Diş Hekimliği Fakültesi, Klinik Bilimler Bölümüen_US
dc.description.abstractThe aim of this study was to compare the load-to-failure resistance and optical properties of nano-lithium disilicate (NLD) with lithium disilicate (LDS) and zirconia-reinforced lithium silicate (ZLS) in different aging processes. Thirty crowns were milled from NLD, LDS, and ZLS (n = 10). All crowns were subjected to thermomechanical aging and loaded until catastrophic failure. Ten specimens from each material were prepared in two different thicknesses (0.7 mm and 1.5 mm, n = 5), and color coordinates were measured before and after coffee thermocycling. Color differences (Delta E00) and relative translucency parameter (RTP) were calculated. Data were analyzed by using ANOVA and Bonferroni-corrected t-tests (alpha = 0.05). ZLS had the highest load-to-failure resistance (p <= 0.002), while the difference between LDS and NLD was nonsignificant (p = 0.776). The interaction between material type and thickness affected Delta E00 (p < 0.001). Among the 0.7 mm thick specimens, ZLS had the lowest Delta E00 (p < 0.001). Furthermore, 1.5 mm thick ZLS had lower Delta E00 than that of 1.5 mm thick LDS (p = 0.036). Other than ZLS (p = 0.078), 0.7 mm thick specimens had higher Delta E00 (p < 0.001). The interaction between material type, thickness, and thermocycling affected RTP (p < 0.001). Thinner specimens presented higher RTP (p < 0.001). NLD and LDS had higher RTP than ZLS (p <= 0.036). However, 0.7 mm thick specimens had similar RTP after coffee thermocycling (p >= 0.265). Coffee thermocycling reduced the RTP values of 0.7 mm thick NLD (p = 0.032) and LDS (p = 0.008). NLD may endure the occlusal forces present in the posterior region. However, long-term coffee consumption may impair the esthetics of restorations particularly when thin NLD is used.en_US
dc.identifier.citationDonmez, M. B., Olcay, E. O., Demirel, M. (2022). Load-to-failure resistance and optical characteristics of nano-lithium disilicate ceramic after different aging processes. Materials, 15(11).en_US
dc.identifier.doi10.3390/ma15114011en_US
dc.identifier.issn1996-1944en_US
dc.identifier.issue11en_US
dc.identifier.scopus2-s2.0-85131962736en_US
dc.identifier.scopusqualityQ2en_US
dc.identifier.urihttps://doi.org/10.3390/ma15114011
dc.identifier.urihttps://hdl.handle.net/20.500.12713/2941
dc.identifier.volume15en_US
dc.identifier.wosWOS:000808696200001en_US
dc.identifier.wosqualityQ2en_US
dc.indekslendigikaynakWeb of Scienceen_US
dc.indekslendigikaynakScopusen_US
dc.indekslendigikaynakPubMeden_US
dc.institutionauthorDönmez, Mustafa Borga
dc.language.isoenen_US
dc.publisherMDPIen_US
dc.relation.ispartofMATERIALSen_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US
dc.rightsinfo:eu-repo/semantics/openAccessen_US
dc.subjectColor Stabilityen_US
dc.subjectLoad-to-Failure Resistanceen_US
dc.subjectNano-Lithium Disilicateen_US
dc.subjectRelative Translucency Parameteren_US
dc.titleLoad-to-failure resistance and optical characteristics of nano-lithium disilicate ceramic after different aging processesen_US
dc.typeArticleen_US

Dosyalar

Orijinal paket
Listeleniyor 1 - 1 / 1
Yükleniyor...
Küçük Resim
İsim:
materials-15-04011-v2.pdf
Boyut:
2.27 MB
Biçim:
Adobe Portable Document Format
Açıklama:
Tam Metin / Full Text
Lisans paketi
Listeleniyor 1 - 1 / 1
Küçük Resim Yok
İsim:
license.txt
Boyut:
1.44 KB
Biçim:
Item-specific license agreed upon to submission
Açıklama: